WL 1.6722-100 Aerospace; case-hardening nickel-chromium-molybdenum steel with approx. 0,15 C, 4 Ni, 1 Cr, 0,2 Mo, comsumable electrode remelted; bars and forgings; design and production data, conversion. Формат поставки-PDF. Язык стандарта-Немецкий, Английский
Другие Стандарты WL
WL 1.4454-1 Aerospace series - Stainless and heat resisting austenitic chromium-manganese-nickel stee...
WL 1.8544-1 Aerospace series - Nitriding chromium-aluminium-molybdenum steel with approx. 0,34 C - 1,...
WL 1.4554-100 Aerospace series - Stainless austenitic chromium-nickel steel with approx. 0,05 C - 19 Cr...
WL 1.4014-1 Aerospace series - Stainless heat treatable chromium steel with approx. 0,2 C - 13 Cr - P...
WL 1.4939-2 High temperature heat-treatable chromium-nickel-molybdenum steel with about 0.1 C-12...
WL 1.4933 Beiblatt 1 High temperature heat-treatable chromium-nickel-molybdenum steel with about 0...