WL 1.6974-1 Aerospace; high-strength hardened and tempered nickel-cobalt steel with approx. 0,3 C, 8 Ni, 4,5 Co, 1 Cr, 1 Mo, consumable electrode remelted; bars and forgings. Формат поставки-PDF. Язык стандарта-Немецкий, Английский
Другие Стандарты WL
WL 1.7214 Beiblatt 1 Weldable heat-treatable chromium-molybdenum steel with about 0.25C-1Cr-0.2Mo;...
WL 1.5934 Beiblatt 1 Case-hardening chromium-nickel steel with about 0,18 C, 2 Cr, 2 Ni; rods and ...
WL 1.4314-4 Aerospace series - Stainless austenitic chromium-nickel steel with approx. 0,05 C - 18 Cr...
WL 1.4943-2 Aerospace; heat-resisting precipitation-hardening nickel-chromium-titanium steel with appr...
WL 1.6657-1 Aerospace; case-hardening nickel-chromium-molybdenum steel with approx. 0,14 C, 3 Ni, 1 Cr...
WL 1.6722-1 Aerospace; case-hardening nickel-chromium-molybdenum steel with approx. 0,15 C, 4 Ni, 1 Cr...